TRIEL® 5722SPU

TPEE

문의하기

TYPICAL DATA OF TRIEL® 5722SPU GRADE

PROPERTY UNIT ASTM METHOD TYPICAL DATA
Physical
Specific Gravity - D792 1.25
Water Absorption (24 hours at 23℃) % D570 0.5
Melt Flow Rate (230도, 2.16kg) g/10min D1238 9
MECHANICAL
Tensile Strength at yield kgf/㎠ D638 425
Tensile Elongation at break % D638 380
Flexural Strength at yield kgf/㎠ D790 370
Flexural Modulus kgf/㎠ D790 10,000
Izod Impact Strength, notched, 23℃ (1/8”) kgf∙㎝/㎝ D256 12
Hardness (Shore D) Shore D 72
THERMAL
HDT, 4.6 ㎏f/㎠ 130
ELECTRICAL
OTHERS
※The figures listed in this table are typical values obtained under the standard test methods and may not be applicable for products that are under different application condition.

PROCESSING GUIDE FOR TRIEL® 5722SPU GRADE

General processing conditions for TRIEL® 5722SPU are shown below.
Drying prior to processing is essential to ensure desired appearance and property performance.

SPECIFICATION UNIT CONDITIONS
Drying Temperature 110~120
Drying Time hr 3~4
Moisture Content, Max % 0.02
Melt Temperature 210~220
Nozzle Temperature 240~260
Front Temperature 240~260
Middle Temperature 240~260
Rear Temperature 230~240
Mold Temperature 30~50