본문 바로가기 대메뉴 바로가기

TRILFT® LF9031G35

PP + Long Glass Fiber

문의하기

TYPICAL DATA OF TRILFT® LF9031G35 GRADE

PROPERTY UNIT ASTM METHOD TYPICAL DATA
Physical
Specific Gravity - D792 1.10
MECHANICAL
Tensile Strength at yield kgf/㎠ D638 1200.0
Flexural Strength at yield kgf/㎠ D790 1350.0
Flexural Modulus kgf/㎠ D790 63000.0
Izod Impact Strength, notched, 23℃ (1/8”) kgf∙㎝/㎝ D256 25.0
Rockwell Hardness R scale D785 108.0
THERMAL
HDT, 18.6 ㎏f/㎠ ℃ D648 158.0
ELECTRICAL
OTHERS
Mold Shrinkage (3mm thickness) % D955 0.25~0.4
※The figures listed in this table are typical values obtained under the standard test methods and may not be applicable for products that are under different application condition.

PROCESSING GUIDE FOR TRILFT® LF9031G35 GRADE

General processing conditions for TRILFT® LF9031G35 are shown below.
Drying prior to processing is essential to ensure desired appearance and property performance.

SPECIFICATION UNIT CONDITIONS
Drying Temperature ℃ 80~100
Drying Time hr 3~5
Moisture Content, Max % 0.02
Melt Temperature ℃ 220~240
Nozzle Temperature ℃ 230~240
Front Temperature ℃ 220~230
Middle Temperature ℃ 220~230
Rear Temperature ℃ 210~220
Mold Temperature ℃ 40
Screw Speed rpm <50
Vent Depth mm 0.02~0.05